[1] Saadati A, Minagar A, Naseri G, Bahmani A, Malekan M. Synthesis of NiAl-TiC composites from elemental powders by volume combustion method. Materials Science and Technology 2019, 35: 831-838.
[2] Mohammadnezhad M, Shamanian M, Enayati MH, Salehi M, Hoseynian A. Microstructures and properties of NiAl–TiC nanocomposite coatings on carbon steel surfaces produced by mechanical alloying technique. Surface and Coatings Technology 2014, 238: 180-187.
[3] Fan X, Huang W, Zhou X, Zou B. Preparation and characterization of NiAl–TiC–TiB2 intermetallic matrix composite coatings by atmospheric plasma spraying of SHS powders. Ceramics International 2020,
[4] Krasnowski M, Gierlotka S, Ciołek S, Kulik T. Nanocrystalline NiAl intermetallic alloy with high hardness produced by mechanical alloying and hot-pressing consolidation. Advanced Powder Technology 2019, 30: 1312-1318.
[5] Ozdemir O, Zeytin S, Bindal C. A study on NiAl produced by pressure-assisted combustion synthesis. Vacuum 2009, 84: 430-437.
[6] Li B, Gao Y, Hou X, Li C, Guo H, Kang Y, Li Y, Zheng Q, Zhao S. Microstructure, mechanical and tribological properties of NiAl matrix composites with addition of BaO/TiO2 binary oxides. Tribology International 2020, 144: 106108.
[7] Riyadi TWB, Zhang T, Marchant D, Zhu X. NiAl–TiC–Al2O3 composite formed by self-propagation high-temperature synthesis process: Combustion behaviour, microstructure, and properties. Journal of Alloys and Compounds 2019, 805: 104-112.
[8] Zarezadeh Mehrizi M, Momeni MR, Beygi R, Eisaabadi B G, Kim B-H, Kim S-K. Reaction pathway of NiAl/WC nanocomposite synthesized from mechanical activated NiAlWC powder system. Ceramics International 2019, 45: 11833-11837.
[9] Rahaei MB. In-Situ Manufacturing of NiAl-TiC Composites with Three Dimensional (3D) Discrete Particular Network and Bi-Continuous Microstructures. Advanced Powder Technology 2019, 30: 1025-1033.
[10] Bonetti E, Campari EG, Pasquini L, Sampaolesi E, Scipione G. Mechanical behaviour of NiAl and Ni3Al ordered compounds entering the nano-grain size regime. Nanostructured Materials 1999, 12: 895-898.
[11] Zarezadeh Mehrizi M, Ahmadi S, Beygi R, Asadi M. Fabrication of Cerium Oxide Nanoparticles by Solution Combustion Synthesis and Their Cytotoxicity Evaluation. Russian Journal of Non-Ferrous Metals 2018, 59: 111-116.
[12] Neto ASB, Oliveira AC, Filho JM, Amadeo N, Dieuzeide ML, de Sousa FF, Oliveira AC. Characterizations of nanostructured nickel aluminates as catalysts for conversion of glycerol: Influence of the preparation methods. Advanced Powder Technology 2017, 28: 131-138.
[13] Goudarzi A, Lalianpour A, Zarezadeh Mehrizi M, Beygi R, Eisaabadi B G. Fabrication of NiAl–Al2O3-WC nanocomposite by mechanical alloying and subsequent heat treatment. Ceramics International 2019, 45: 19049-19054.
[14] Zarezadeh Mehrizi M, Jalali H, Beygi R, Velashjerdi M. Synthesis of NiAl-TiC nanocomposite during mechanical alloying of Ni–Ti–Al–C powder mixture. Materials Research Express 2019, 6: 125063.
[15] Curfs C, Cano IG, Vaughan GBM, Turrillas X, Kvick Å, Rodrı́guez MA. TiC–NiAl composites obtained by SHS: a time-resolved XRD study. Journal of the European Ceramic Society 2002, 22: 1039-1044.
[16] Zhang H, Zhu H, Huang J, Li J, Xie Z. In-situ TiB2-NiAl composites synthesized by arc melting: Chemical reaction, microstructure and mechanical strength. Materials Science and Engineering: A 2018, 719: 140-146.
[17] Xie R, Li D, Yang G, Li C. The influence of zirconium carbide addition on oxidation behaviour of NiAl coatings prepared by cold spraying of ball-milled Ni–Al alloy powder. Materials Science and Technology 2013, 29: 1125-1129.
[18] Chawake N, Koundinya NTBN, Kottada RS. Verification of correlation between densification during spark plasma sintering and compressive creep of ultrafine-grained in-situ Al2O3-reinforced B2 aluminide matrix composites. Journal of Alloys and Compounds 2018, 735: 1921-1930.
[19] Yeh CL, Ke CY, Chen YC. In situ formation of TiB2/TiC and TiB2/TiN reinforced NiAl by self-propagating combustion synthesis. Vacuum 2018, 151: 185-188.
[20] Zarezadeh Mehrizi M, Mostaan H, Beygi R, Rafiei M, Abbasian AR. Reaction Pathways of Nanocomposite Synthesized in-situ from Mechanical Activated Al–C–TiO2 Powder Mixture. Russian Journal of Non-Ferrous Metals 2018, 59: 117-122.
[21] Chen L, Sun Y, Li L, Ren Y, Ren X. In situ TiC/Inconel 625 nanocomposites fabricated by selective laser melting: Densification behavior, microstructure evolution, and wear properties. Applied Surface Science 2020, 145981.
[22] Aghamohammadi H, Heidarpour A, Jamshidi R, Ghasemi S. Study on the chemical stability of the synthesized TiCx in Ti-Al-C system after immersion in the HF + H2O2 solution. Advanced Powder Technology 2019, 30: 393-398.
[23] Zarezadeh Mehrizi M, Saidi A, Shamanian M, Eslami HR. Combustion synthesis of Fe–Al/TiC composite powders and effect of Al content on its characteristics. Powder Metallurgy 2011, 54: 400-403.
[24] Zarezadeh Mehrizi M, Beygi R, Eisaabadi B G, Velashjerdi M, Nematzadeh F. Mechanically activated combustion synthesis of Ti3AlC2/Al2O3 nanocomposite from TiO2/Al/C powder mixtures. Advanced Powder Technology 2019, 30: 311-316.
[25] Mukasyan AS, Rogachev AS, Aruna ST. Combustion synthesis in nanostructured reactive systems. Advanced Powder Technology 2015, 26: 954-976.
[26] Yeh CL, Chen YC. Fabrication of MoSi2–MgAl2O4 in situ composites by combustion synthesis involving intermetallic and aluminothermic reactions. Vacuum 2019, 167: 207-213.
[27] Zhu X, Zhang T, Marchant D, Morris V. The structure and properties of NiAl formed by SHS using induction heating. Materials Science and Engineering: A 2011, 528: 1251-1260.
[28] Yeh CL, Su SH, Chang HY. Effects of TiC addition on combustion synthesis of NiAl in SHS mode. Journal of Alloys and Compounds 2005, 398: 85-93.
[29] Biswas A, Roy SK, Gurumurthy KR, Prabhu N, Banerjee S. A study of self-propagating high-temperature synthesis of NiAl in thermal explosion mode. Acta Materialia 2002, 50: 757-773.
[30] Kozhina G, Estemirova S, Pechishcheva N, Murzakaev A, Vovkotrub E, Skrylnik M, Shunyaev K. Joint mechanical activation of MnO2, Fe2O3 and graphite: Mutual influence on the structure. Advanced Powder Technology 2017, 28: 1202-1212.
[31] Boldyrev VV. Mechanochemistry and mechanical activation of solids. Russian Chemical Reviews 2006, 75: 177-189.
[32] Yan S-R, Mehrizi MZ, Foong LK. Synthesis of NiAl-WC composite by the thermal explosion of elemental powders. Ceramics International 2020,
[33] Cai X, Liu Y, Feng P, Jiao X, Zhang L, Wang J. Fe-Al intermetallic foam with porosity above 60 % prepared by thermal explosion. Journal of Alloys and Compounds 2018, 732: 443-447.
[34] Trevino R, Maguregui E, Perez F, Shafirovich E. Mechanically activated SHS of Nb5Si3 and Nb5Si3/Nb composites. Journal of Alloys and Compounds 2020, 826: 154228.
[35] Qanavatian H, Zarezadeh Mehrizi M, Raoufi M. Synthesis of Fe3 Al–TiC-SiC Nanocomposite by Mechanical Alloying of FeSiTiO3–Al–C Powders. Silicon 2019, 11: 1497-1503.
[36] Ozdemir O, Zeytin S, Bindal C. Characterization of two-phase nickel aluminides produced by pressure-assisted combustion synthesis. Vacuum 2007, 82: 311-315.
[37] Rosiński M, Michalski A. Nanocrystalline NiAl-TiC Composites Sintered by the Pulse Plasma Method. Solid State Phenomena 2006, 114: 233-238.
[38] Zhu X, Zhang T, Marchant D, Morris V. Combustion synthesis of TiC–NiAl composite by induction heating. Journal of the European Ceramic Society 2010, 30: 2781-2790.