[1] Song, HH.; Zhang, ZZ.; Luo, ZZ. Surf. Effects of solid lubricants on friction and wear behaviors of the phenolic coating under different friction conditions. Coat. Technol. 2006, 201,2760.
[2] Sahebali Manafi, Syed Rahim Kiahosseini. Polytetrafluoroethylene/nanoclay composite as anti-wearing compound. Iran. Polym. J. 2020, 29:25–35.
[3] Dapeng Gu, Changsheng Duan, Bingli Fan, et al. Tribological properties of hybrid PTFE/Kevlar fabric composite in vacuum. Tribol. Int. 2016, 103:423–431.
[4] Shiguang Peng, Lin Zhang, Guoxin Xie, et al. Friction and wear behavior of PTFE coatings modified with polymethyl methacrylate. Compos. Part. B-ENG. 2019, 172:316–322.
[5] You Shi, Sheng Tai Zhou, Zheng Guang Heng, et al. Interlocking structure formed by multiscale carbon fiber−polytetrafluoroethylene fiber hybrid significantly enhances the friction and wear properties of polyphenylene sulfide based composites. Ind. Eng. Chem. Res. 2019, 58, 36, 16541–16551.
[6] Zhao, Q.; Bahadur, S. Investigation of the Transition State in the wear of Polyphenylene sulfide sliding against steel. Tribol. Lett. 2002, 12(1), 23.
[7] Lin, L.; Schlarb, A. K. The roles of rigid particles on the friction and wear Behavior of short carbon fiber reinforced PBT hybrid materials in the Absence of Solid Lubricants. Tribol. Int. 2018, 119, 404−410.
[8] Qi, H.; Zhang, L.; Zhang, G.; Wang, T.; Wang, Q. Comparative study of tribochemistry of ultrahigh molecular weight polyethylene, polyphenylene sulfide and polyetherimide in tribo-composites. J. Colloid Interface Sci. 2018, 514, 615−624.
[9] Shicheng YAN, Yahong XUE, Yahui HU, Shoujun WANG. Thermal, mechanical, and tribological properties of sodium–montmorillonite-nanoparticle-reinforced polyethersulfone and polytetrafluoroethylene ternary composites. Friction, 2020, DOI: 10.1007/s40544-019-0343-x.
[10] Jiaxin Ye, Wei Sun, Yan Zhang, Xiaojun Liu, Kun Liu. Measuring evolution of transfer film–substrate interface using low wear Alumina PTFE. Tribology Letters. 2018, 66:100.
[11] Krick, B. A.; Pitenis, A. A.; Harris, K. L.; Junk, C. P.; Sawyer, et al. Ultralow Wear Fluoropolymer Composites: Nanoscale Functionality from Microscale Fillers. Tribol. Int. 2016, 95, 245−255.
[12] Qinglun Che, Ga Zhang, Ligang Zhang, et al. Switching brake materials to extremely wear-resistant self-lubrication materials via tuning interface nanostructures. ACS Appl. Mater. Interfaces. 2018, 10, 19173−19181.
[13] Jin-Oh, C., Sang-Ryul, G, Jeong-Hee, K., Hyang-Rae, K. and Hee-Bum, C. “Conditions for transfer film formation and its effect on friction coefficients in nao friction materials containing various abrasive components”, Int. J. Precis. Eng. Man. 2018, 19, 7:1011-1017.
[14] Junyuan MAO, Guangyan CHEN, Jun ZHAO, Yongyong HE, Jianbin LUO. An investigation on the tribological behaviors of steel/copper and steel/steel friction pairs via lubrication with a grapheme additive. Friction, 2020, DOI: 10.1007/s40544-019-0327-x.
[15] M.T. Masood, E.L. Papadopoulou, J.A. Heredia-Guerrero, I.S. Bayer, A, et al. Graphene and polytetrafluoroethylene synergistically improve the tribological properties and adhesion of nylon 66 coatings. Carbon. 2017, 123, 26.
[16] Junya Yuan, Zhaozhu Zhang, Mingming Yang, et al. Combined Effects of Interface Modification and Nano-Reinforcement via Nano-Enhanced Interphase in Hybrid-Fabric Composites for Tribological Applications. Polymer Composites. 2019, 40, 9: 3383-3392.
[17] Qiufeng Wang, Yunxia Wang, Hongling Wang, et al. Comparative study of the effects of nano-sized and micro-sized CF and PTFE on the thermal and tribological properties of PEEK composites. Polym. Adv. Technol. 2018, 29, 2:896–905.
[18] C.B. Wanga, M.F. Yan, Y. Wang. The influence of metal surface composition on the tribological properties of filled PTFE/steel couples. Tribol. Int. 2004, 37:645–650.
[19] Ben Wang, Wei Han, Yueke Ming, et al. Preparation and Tribological Study of Graphene Coating on Glass Fiber-Reinforced Composite Using Modified Percolating-Assisted Resin Film Infusion Method. Materials. 2020, 13, 851.
[20] Qiaoqin Guo, Yongchun Guo, Ding Guo, et al. Microstructure and properties of the Cp/AlSn coatings deposited by magnetron sputtering/multi-arc ion plating. Surf. Coat. Tech. 2020, 384: 125303.
[21] Mengjiao Wang, Hao Liu, Yunxia Wang, et al. Stable lubrication in air and vacuum of GO-Al3+ coating via strong chemical bonding and reactive sites passivation by aluminum ions. Carbon. 2020, 160:247-254.
[22] Jasbir Singh Kunnan Singh, Yern Chee Ching, De Shin Liu, et al. Effects of PTFE micro-particles on the fiber-matrix interface of polyoxymethylene/glass fiber/polytetrafluoroethylene composites. Materials. 2018, 11, 2164.
[23] Yingyi Liu, Nuo Xu, Yuan Wang. Preparation and tribological properties of hybrid PTFE/Kevlar fabric self-lubricating composites. Surf. Coat. Tech. 2019, 361:196–205.
[24] Xiaoshuang Xionga, Shirley Z. Shend, Nazmul Alamd, et al. Mechanical and abrasive wear performance of woven flax fabric/polyoxymethylene composites. Wear, 2018, 414–415:9–20.
[25] Dapeng Gu, Longxiao Zhang, Suwen Chen, et al. Reciprocating sliding wear of hybrid PTFE/Kevlar fabric composites along different orientations. RSC Adv. 2018, 8, 20877–20883.
[26] Enhanced tribological performance of hybrid polytetrafluoroethylene/Kevlar fabric composite filled with milled pitch-based carbon fibers. J. Appl. Polym. Sci. 2018, 135, 19, 46269.
[27] Shiguang Peng, Lin Zhang, Guoxin Xie, et al. Friction and wear behavior of PTFE coatings modified with polymethyl methacrylate. Compos. Part. B-ENG. 2019, 172: 316–322.
[28] Jinbang Li, Shuaishuai Zeng, Shuo Liu, Ningning Zhou, Tao Qing. Tribological properties of textured stator and PTFE-based material in travelling wave ultrasonic motors. Friction. 2020, 8, 2: 301–310.
[29] Suvrat Bhargava, Mary E. Makowiec, Thierry A. Blanchet. Wear reduction mechanisms within highly wear-resistant graphene and other carbon-filled PTFE nanocomposites. Wear. 2020, 444-445: 203163.
[30] Song LI, Chunjian DUAN, Xiao LI, et al. The effect of different layered materials on the tribological properties of PTFE composites. Friction. 2020, 8(3): 542–552.
[31] Ting Xie, Shihao Feng, Zhaoming Yan, Tingting Yang. Tribo-magnetization of the PTFE composites containing ferromagnetic fillers of Fe, Co, or Ni. Wear. 2019, 424–425:233–245.
[32] M.D. Placette, S. Roy, D. White, et al. The effect of surface roughness orientation on PEEK (polyetheretherketone) transfer film volume in multi-directional and linear sliding. Wear. 2019, 426–427:1345–1353.
[33] Ting Xie, Junjie Lai and Huaping Yang. Simulation of effect of counterface roughness on the friction transfer and wear of PTFE sliding against steel. Ind. Lubr. Tribol. 2019, 71, 9:1086–1092.
[34] Fuzhi Song, Zenghui Yang, Gai Zhao, et al. Tribological performance of filled PTFE-based friction material for ultrasonic motor under different temperature and vacuum degrees. J. Appl. Polym. Sci. 2017, 134, 39:45358.
[35] E-L. Yang and J.-P. Hirvonen. Effect of temperature on the transfer film formation in sliding contact of PTFE with stainless steel. Wear. 1991, 146:367-376.
[36] Annelise Jean-Fulcrand, Marc A. Masen, Tim Bremner, Janet S.S. Wong. High temperature tribological properties of polybenzimidazole. Polymer. 2017, 128: 159-168.
[37] Ruoxuan Huang, Siqi Ma, Meidi Zhang, et al. Wear Evolution of the Glass Fiber-Reinforced PTFE under Dry Sliding and Elevated Temperature. Materials. 2019, 12, 1082.
[38] Kian Bashandeh, Pixiang Lan, Jacob L. Meyer, Andreas A. Polycarpou. Tribological Performance of Graphene and PTFE Solid Lubricants for Polymer Coatings at Elevated Temperatures. Tribol. Lett. 2019, 67:99.
[39] Leyu Lin, Xian Qiang Pei, Roland Bennewitz, Alois K. Schlarb. Tribological Response of PEEK to Temperature Induced by Frictional and External Heating. Tribol. Lett. 2019, 67:52.
[40] T. Onodera, J. Nunoshige, K. Kawasaki, K. Adachi, K. Kurihara, M. Kubo, Structure and function of transfer film formed from PTFE/PEEK polymer blend, J. Phys. Chem. C. 2017, 121: 14589–14596.
[41] E. Padenko, L.J. van Rooyen, J. Karger-Kocsis, Transfer film formation in PTFE/oxyfluorinated graphene nanocomposites during dry sliding, Tribol. Lett. 65 (2017) 1–11.
[42] J. Ma, X. Qi, Y. Dong, Y. Zhao, Q. Zhang, B. Fan, Y. Yang, Transfer film formation mechanism and tribochemistry evolution of a low-wear polyimide/mesoporous silica nanocomposite in dry sliding against bearing steel, Tribol. Int. 2018, 120: 233–242.
[43] M. Tokoro, Y. Aiyama, M. Masuko, A. Suzuki, H. Ito, K. Yamamoto, Improvement of tribological characteristics under water lubrication of DLC-coatings by surface polishing, Wear. 2009, 267:2167–2172.
[44] Y. Yamamoto, M. Hashimoto, Friction and wear of water lubricated PEEK and PPS sliding contacts Part 2. Composites with carbon or glass fibre, Wear. 2004, 257:181–189.
[45] JianzhangWang, Fengyuan Yan, Qunji Xue. Tribological behavior of PTFE sliding against steel in sea water. Wear. 2009, 267:1634–1641.
[46] T.J. Joyce, P. Thompson, A. Unsworth. The wear of PTFE against stainless steel in a multi-directional pin-on-plate wear device. Wear. 2003, 255:1030–1033.
[47] Diana R. Haidar, K. Istiaque Alam, David L. Burris. Tribological insensitivity of an ultralow-wear Poly(etheretherketone)−Polytetrafluoroethylene polymer blend to changes in environmental moisture. J. Phys. Chem. C. 2018, 122, 5518−5524.
[48] Qiaoqin Guo, Yongchun Guo, Ding Guo. Microstructure and properties of the Cp/AlSn coatings deposited by magnetron sputtering/multi-arc ion plating. Surf. Coat. Tech. 2020.384: 125303.
[49] Jian Ma, Xiaowen Qi, Yu Dong, et al. Transfer film formation mechanism and tribochemistry evolution of a low-wear polyimide/mesoporous silica nanocomposite in dry sliding against bearing steel. Tribol. Int. 2018, 120:233–242.
[50] Houbao Liu , Xinqing Su, Jie Tao, et al. Influence of cenosphere on tribological properties of short carbon fiber reinforced PEEK composites. J. Appl. Polym. Sci. 2019,136, 12, 47245.
[51] J. Zhao, J.Y. Mao, Y.R. Li, Y.Y. He, J.B. Luo. Friction-induced nano-structural evolution of graphene as a lubrication additive. Appl. Surf. Sci. 2018, 434: 21–27.
[52] Satyaprasad, Jain, SK. Deposition of superhydrophobic nanostructured Teflon-like coating using expanding plasma arc. Applied Surface Science, 2007, 253(12): 5462-5466.
[53] A. J. Wood, M. J. Cozad, D. A. Grant, et al. Materials characterization and histological analysis of explanted polypropylene, PTFE, and PET hernia meshes from an individual patient. J. Mater. Sci. 2013, 24:1113–1122.
[54] Dhanabalan, V, Xavier, KAM , Eppen, S, et al. Characterization of chitin extracted from enzymatically deproteinized Acetes shell residue with varying degree of hydrolysis. Carbohyd. Polym.2021, 1, 253:117203.
[55] Zheng, Wei, Halim, Joseph, El Ghazaly, Ahmed, et al. Flexible Free-Standing MoO3/Ti3C2Tz MXene Composite Films with High Gravimetric and Volumetric Capacities. Adv. Sci. 2021, 8, 3: 2003656.